| SL
5195 Resin |
|
| Typical
Properties: Liquid Resin SL 5195
|
| Measurement |
Condition |
Value |
| Appearance |
  |
Clear |
| Density |
@
25° C (77° F) |
1.16
g/cc |
| Viscosity |
@
25° C (77° F)
@ 30° C (86° F) |
230
cps
180 cps |
| Penetration
depth (Dp)* |
|
5.2
mils |
| Critical
exposure (Ec)* |
|
13.1
mJ/cm² |
|
|
| Typical
Properties: Post-Cured Part** |
| Measurement |
Method |
Value |
| Tensile
strength |
ASTM
D 638 |
46.5
Mpa (6,740 psi) |
| Tensile
modulus |
ASTM
D 638 |
2,090
Mpa (303 ksi) |
| Elongation
at break |
ASTM
D 638 |
11-22% |
| Flexural
strength |
ASTM
D 790 |
49.3
Mpa (7,150 psi) |
| Flexural
modulus |
ASTM
D 790 |
1,628
Mpa (236 ksi) |
| Impact
strength, notched |
ASTM
D 256 |
1.0
ft-lbs/in |
| Hardness,
Shore D |
DIN
53505 |
83
Shore D |
| Heat
deflection temp |
ASTM
D 648 |
|
|
@
66 psi (UV postcure) |
47°
C (117° F) |
|
|
*
For reference only. Actual number may vary by machine.